JPH0244274B2 - - Google Patents
Info
- Publication number
- JPH0244274B2 JPH0244274B2 JP61315237A JP31523786A JPH0244274B2 JP H0244274 B2 JPH0244274 B2 JP H0244274B2 JP 61315237 A JP61315237 A JP 61315237A JP 31523786 A JP31523786 A JP 31523786A JP H0244274 B2 JPH0244274 B2 JP H0244274B2
- Authority
- JP
- Japan
- Prior art keywords
- weight
- cement
- coating
- film
- resin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Aftertreatments Of Artificial And Natural Stones (AREA)
- Curing Cements, Concrete, And Artificial Stone (AREA)
- Paints Or Removers (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP61315237A JPS63162564A (ja) | 1986-12-25 | 1986-12-25 | 凹凸表面を有するセメント製品の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP61315237A JPS63162564A (ja) | 1986-12-25 | 1986-12-25 | 凹凸表面を有するセメント製品の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS63162564A JPS63162564A (ja) | 1988-07-06 |
JPH0244274B2 true JPH0244274B2 (en]) | 1990-10-03 |
Family
ID=18063028
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP61315237A Granted JPS63162564A (ja) | 1986-12-25 | 1986-12-25 | 凹凸表面を有するセメント製品の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS63162564A (en]) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP4540154B2 (ja) * | 1999-10-25 | 2010-09-08 | 新日鐵化学株式会社 | コンクリート構造物用下地調整材組成物およびその製造方法 |
JP4850747B2 (ja) * | 2007-02-21 | 2012-01-11 | 太平洋セメント株式会社 | セメント質硬化体 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5723665A (en) * | 1980-07-18 | 1982-02-06 | Pilot Pen Co Ltd:The | Water-based ink composition for ink jet recording |
JPS6019940A (ja) * | 1983-07-12 | 1985-02-01 | Mazda Motor Corp | エンジンの制御装置 |
-
1986
- 1986-12-25 JP JP61315237A patent/JPS63162564A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS63162564A (ja) | 1988-07-06 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP3041189B2 (ja) | 水性下地調整材とそれを用いた建築物外壁仕上方法 | |
JP2003300009A (ja) | 模様面の形成方法 | |
JPS6072964A (ja) | 給油施設等の防火壁の塗装仕上げ方法 | |
JP2018065998A (ja) | 水性被覆材 | |
JP2024133371A (ja) | 2液型の水性被覆材 | |
JP2709521B2 (ja) | 無機水硬性板材の製造方法 | |
JPH0244274B2 (en]) | ||
JPH0116872B2 (en]) | ||
JPS6113506B2 (en]) | ||
JP3165607B2 (ja) | コンクリート表面厚付け岩石調化粧工法 | |
JP5090703B2 (ja) | 水性塗材 | |
JPS5946913B2 (ja) | 着色セメント瓦の製造方法 | |
JPS5914427B2 (ja) | 着色セメント瓦の製造方法 | |
JP2505387B2 (ja) | エマルション塗膜形成方法 | |
JPS63210084A (ja) | 凹凸表面を有するセメント製品の製造方法 | |
JPS6320800B2 (en]) | ||
JP6171060B1 (ja) | ポリマーセメント系組成物 | |
JP7603477B2 (ja) | 被膜形成方法 | |
JP2004149776A (ja) | 骨材着色用組成物、着色骨材及び外装用クリヤー仕上げ塗装板 | |
JP4637471B2 (ja) | 水性塗料組成物 | |
JPS5914428B2 (ja) | 着色セメント瓦の製造方法 | |
JPS61141684A (ja) | 塗装化粧板の製造方法 | |
US4053664A (en) | Low temperature glazing method | |
JP2023180244A (ja) | 水系シーラー組成物およびシーラー塗膜付き無機質基材 | |
JPS634874B2 (en]) |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
LAPS | Cancellation because of no payment of annual fees |